CuZr --UNS.C15000 Zirconium Copper Alloys

Build Your Online Product Catalogs?



Description
Product Name: CuZr --UNS.C15000 Zirconium Copper Alloys
Supply Ability: 30Tons/month
Related proudcts
Specifications UNS.C15000
Price Term: CFR
Port of loading: Xiamen
Minimum Order 300kgs
Unit Price:

CuZr---UNS.C15000 Zirconium Copper is an excellent and unique copper alloy with high electrical conductivity, hardness, and ductility, moderate strength, and excellent resistance to softening at elevated temperatures. The addition of 0.15% zirconium (Zr) to copper results in a heat treatable copper alloy which may be solution treated and subsequently aged to produce these desirable properties. Rod is supplied from the mill in the fully aged and drawn condition so no further heat treatment is required by the fabricator. The softening temperature of properly heat treated C15000 rod exceeds 500℃ as co***red to unalloyed, pure copper which softens at 200℃ and silver bearing coppers which soften at 350℃.

Typical Application for C15000 Zirconium Copper Alloys:
Electrical Industry: Resistance Welding Electrodes, Circuit Breaker Switches, Stud Bases for Power Transmitters, Rectifiers, Diodes, Switches, Commutators
Consumer: Rod Extensions, Pencil-type, Light Soldering Guns, Tips
Industrial: Connectors, Solderless Wrapped, Welding Wheels, Resistance Welding Tips
Available Sizes:
Custom Diameter & Sizes, Random Mill lengths
Available Products (forms):
Round bars, Flat bars, Square bars, Rectangular bars, Hexagon bars, Plates
Custom shapes are available upon request.
Chemical Composition:
Zr: 0.15-0.20%
Cu: Balance
Note: Copper plus additions equal 99.90% minimum.
Typical Physical Properties:

Density at 68¡ãF: 0.321 Lbs./In.3
Specific Gravity: 8.89
Melting Point (Liquidus): 1080℃ (1976¡ãF)
(Solidus): 980℃ (1796¡ãF)
Coefficient of Thermal Expansion per ¡ãF: 9.4 x 10-6 (68-212¡ãF)
9.8 x 10-6 (68-572¡ãF)
11.2 x 10-6 (68-1200¡ãF)
Electrical Conductivity at 68¡ãF (volumetric): 85-95% IACS (aged and drawn)
55-72% IACS (solution annealed)
Thermal Conductivity Btu/ft.2/ft./hr./¡ãF at 68¡ãF: 212
Modulus of Elasticity - Tension: 18,700 ksi
Note:
1). the units are based upon US Customary.
2). the typical physical properties app

Contact Us
Company: ALB(Xiamen)Material Co***ny Limited
Contact: Ms. Jane Zhang
Address: Rm801-803, ZiAn Pavilion,No.186, Huarong Road, Huli District
Postcode: 361006
Tel: 86-0592-5607665
Fax: 86-0592-5607657
E-mail:         


Copyright© ALB(Xiamen)Material Co***ny Limited All Rights Reserved.
Tel : 86-0592-5607665 Fax : 86-0592-5607657
Powered by 86exporter.com